Passionate about your pursuit? TyTek is here to help  Why Ferrite Magnets are pulling manufacturers in…  Taking the load  Will Rare Earth Become Rarer Still?  GDPR Update Announcement  Finding the Right Formula for the Future of Magnetics  New trauma response system will help to save lives in the event of a mass casualty incident  Create Domestic Bliss with our Ten Magnetic Tricks  Five Life-saving Benefits of Ptensys  Seven Weird and Wonderful Ways we use Magnets   

Magnets

Sintered Alnico Magnets from TyTek Industries

SA-2

Grade: Sintered Alnico 2
Magnetic Properties 25°C C.G.S. Units S.I. Units
Residual Induction (Br) 6,600 Gauss 660 mT
Coercive Force (Hc) 550 Oersteds 44 kA/m
Intrinsic Coercive Force (Hci) 550 Oersteds 44 kA/m
Maximum Energy Product (BHmax) 1.40 MGOe 11.1 kJ/m³
Temperature Coefficient of Br -0.03%/°C
Temperature Coefficient of Hci -0.02%/°C
Relative Recoil Permeability 5.6 G/Oe
Curie Temperature 810°C

 

Physical Properties
Density 6.8 g/cm³
Thermal Expansion Coefficient 12.4 x 10-6 /°C
Electrical Resistivity* 68  Ωcm/cm²
Tensile Strength* 450 N/mm²
Flexural Strength* 480 N/mm²
Rockwell Hardness 45

*Reference Values dependent on size, shape, density, orientation and other characteristics

 

SA-5

Grade: Sintered Alnico 5
Magnetic Properties 25°C C.G.S. Units S.I. Units
Residual Induction (Br) 10,800 Gauss 1,080 mT
Coercive Force (Hc) 600 Oersteds 48 kA/m
Intrinsic Coercive Force (Hci) 600 Oersteds 48 kA/m48 kA/m
Maximum Energy Product (BHmax) 3.8 MGOe 30 kJ/m³
Temperature Coefficient of Br -0.02%/°C
Temperature Coefficient of Hci -0.02%/°C
Relative Recoil Permeability 5.2 G/Oe
Curie Temperature 900°C

 

Physical Properties
Density 7.0 g/cm³
Thermal Expansion Coefficient 11.3 x 10-6 /°C
Electrical Resistivity* 50  Ωcm/cm²
Tensile Strength* 350 N/mm²
Flexural Strength* 415 N/mm²
Rockwell Hardness 50

*Reference Values dependent on size, shape, density, orientation and other characteristics

SA-8

Grade: Sintered Alnico 8
Magnetic Properties 25°C C.G.S. Units S.I. Units
Residual Induction (Br) 7,000 Gauss 800 mT
Coercive Force (Hc) 1,700 Oersteds 135 kA/m
Intrinsic Coercive Force (Hci) 1,700 Oersteds 135 kA/m
Maximum Energy Product (BHmax) 5.0 MGOe 39.8 kJ/m³
Temperature Coefficient of Br -0.025%/°C
Temperature Coefficient of Hci -0.01%/°C
Relative Recoil Permeability 1.8 G/Oe
Curie Temperature 860°C

 

Physical Properties
Density 7.0 g/cm³
Thermal Expansion Coefficient 11 x 10-6 /°C
Electrical Resistivity* 54  Ωcm/cm²
Tensile Strength* 380 N/mm²
Flexural Strength* 380 N/mm²
Rockwell Hardness 53

*Reference Values dependent on size, shape, density, orientation and other characteristics

 