The global supply chain in 2023: what to watch out for  What are rare earth magnets and their applications? TyTek Industries explains…  What factors will be shaping the future of the global supply chain?  3 things to think about as a small business when you’re looking to scale up  Rare Earth Magnets are in high demand and Biden decides against restricting imports  What current challenges could affect the global supply chain moving forwards?  There is light amongst the darkness as Manufacturers are staying positive during the post-pandemic crisis  UK logistics giant, EV cargo says that shipping challenges will last for years to come  Are you making the most of innovation as a manufacturing business?  We’re over half way through 2022, what’s the current state of the global supply chain?  

Magnets

Cast Alnico Magnets from TyTek Industries

CA-2

Grade: Cast Alnico 2
Magnetic Properties 25°C C.G.S. Units S.I. Units
Residual Induction (Br) 7,200 Gauss 720 mT
Coercive Force (Hc) 560 Oersteds 45 kA/m
Intrinsic Coercive Force (Hci) 500 Oersteds 45 kA/m
Maximum Energy Product (BHmax) 1.60 MGOe 12.7 kJ/m³
Temperature Coefficient of Br -0.03%/°C
Temperature Coefficient of Hci -0.02%/°C
Relative Recoil Permeability 6.2 G/Oe
Curie Temperature 810°C
Physical Properties
Density 7.0 g/cm³
Thermal Expansion Coefficient 13 x 10-6 /°C
Electrical Resistivity* 65  Ωcm/cm²
Tensile Strength* 20 N/mm²
Flexural Strength* 50 N/mm²
Rockwell Hardness 45

*Reference Values dependent on size, shape, density, orientation and other characteristics

CA-3

Grade: Cast Alnico 3
Magnetic Properties 25°C C.G.S. Units S.I. Units
Residual Induction (Br) 7,000 Gauss 700 mT
Coercive Force (Hc) 475 Oersteds 38 kA/m
Intrinsic Coercive Force (Hci) 500 Oersteds 40 kA/m
Maximum Energy Product (BHmax) 1.60 MGOe 12.7 kJ/m³
Temperature Coefficient of Br -0.03%/°C
Temperature Coefficient of Hci -0.02%/°C
Relative Recoil Permeability 5.1 G/Oe
Curie Temperature 810°C

 

Physical Properties
Density 6.9 g/cm³
Thermal Expansion Coefficient 13 x 10-6 /°C
Electrical Resistivity* 60  ?cm/cm²
Tensile Strength* 80 N/mm²
Flexural Strength* 160 N/mm²
Rockwell Hardness 45

*Reference Values dependent on size, shape, density, orientation and other characteristics

CA-5

Grade: Cast Alnico 5
Magnetic Properties 25°C C.G.S. Units S.I. Units
Residual Induction (Br) 12,500 Gauss 1,250 mT
Coercive Force (Hc) 640 Oersteds 51 kA/m
Intrinsic Coercive Force (Hci) 640 Oersteds 51 kA/m
Maximum Energy Product (BHmax) 5.50 MGOe 44.0 kJ/m³
Temperature Coefficient of Br -0.02%/°C
Temperature Coefficient of Hci -0.02%/°C
Relative Recoil Permeability 3.7 G/Oe
Curie Temperature 860°C

 

Physical Properties
Density 7.3 g/cm³
Thermal Expansion Coefficient 11.5 x 10-6 /°C
Electrical Resistivity* 47  Ωcm/cm²
Tensile Strength* 40 N/mm²
Flexural Strength* 70 N/mm²
Rockwell Hardness 50

*Reference Values dependent on size, shape, density, orientation and other characteristics

 

CA-8

Grade: Cast Alnico 8
Magnetic Properties 25°C C.G.S. Units S.I. Units
Residual Induction (Br) 8,300 Gauss 830 mT
Coercive Force (Hc) 1,650 Oersteds 131 kA/m
Intrinsic Coercive Force (Hci) 1,650 Oersteds 131 kA/m
Maximum Energy Product (BHmax) 5.50 MGOe 43.8 kJ/m³
Temperature Coefficient of Br -0.025%/°C
Temperature Coefficient of Hci -0.01%/°C
Relative Recoil Permeability 2.0 G/Oe
Curie Temperature 860°C

 

Physical Properties
Density 7.3 g/cm³
Thermal Expansion Coefficient 11 x 10-6 /°C
Electrical Resistivity* 50  Ωcm/cm²
Tensile Strength* 60 N/mm²
Flexural Strength* 205 N/mm²
Rockwell Hardness 56

*Reference Values dependent on size, shape, density, orientation and other characteristics